Catalyst 900 - Nylon Jacket Ink Catalyst
Print on Nylon Jackets With Internationa Coatings Catalyst 900 - Nylon Jacket Ink Catalyst Nylon jacket threads are woven very tightly to resist wind and water, but that also makes it hard for plastisol ink to stick. Nylon jackets need a catalyst you mix into your ink just before you print. It's an adhesive that hardens so your ink has to be used in less than 4 hours. This is not a substitute for heat curing, you still have to cure your plastisol ink according to the manufacturers instructions. Catalyst to Ink Ratios:By Volume = 16 parts of ink color to 1 part of 900 Catalyst. By Weight = 20 parts of ink color to 1 part of 900 Catalyst. Mixing by weight is highly recommended Use ink immediately after mixing Do not under catalyze The mixed ink pot life of mixed ink is 4 to 8 hours Over catalyzation will shorten the life of the ink Store your catalyst bottle upside down in a warm dry area. Moisture in the air makes the catalyst harden. On the shelf, any moisture inside the bo